Why are there differences in the required dry film thicknesses for the same section factor?

Different profile types (open sections or hollow sections) have different heating behaviour. For example, hollow sections heat up faster than open sections (e.g. I sections, H sections) with the same U/A factor. Therefore, the coating thicknesses to be applied are determined according to the building component.

Back To Top
Privacy Overview

This website uses cookies so that we can provide you with the best user experience possible. Cookie information is stored in your browser and performs functions such as recognising you when you return to our website and helping our team to understand which sections of the website you find most interesting and useful.